技术指标如下:
|
MgO% ≥ |
Al2O3% ≥ |
Fe2O3% ≤ |
SiO2% ≤ |
ZrO2% |
显气孔率% ≤ |
体积密度g/cm3 ≥ |
常温耐压强度Mpa ≥ |
0.2MPa荷重软化开始温度°C≥ |
热膨胀率(1200°C) |
热震稳定性 |
导热率(1100°C)
w/mk |
| 1100°C |
950°C |
| 镁铝尖晶石砖 |
| MLS-85A |
85 |
9 |
0.9 |
0.9 |
|
18 |
2.95 |
55 |
1700 |
1.5 |
12 |
100 |
2.8 |
| MLS-93A |
85 |
9 |
1.2 |
1.2 |
|
18 |
2.90 |
50 |
1650 |
1.5 |
12 |
100 |
2.9 |
| MLS-95A |
85 |
9 |
1.5 |
1.5 |
|
19 |
2.85 |
40 |
1600 |
1.5 |
12 |
100 |
3.0 |
| MLS-85B |
89-93 |
5-8 |
0.8 |
0.8 |
|
16-18 |
2.90 |
50 |
1700 |
1.6 |
10 |
80 |
2.8 |
| MLS-93B |
89-93 |
5-8 |
1.0 |
1.0 |
|
16-19 |
2.85 |
40 |
1650 |
1.6 |
10 |
80 |
2.9 |
| MLS-95B |
93-96 |
3-5 |
1.0 |
1.0 |
|
17-19 |
2.85 |
40 |
1650 |
1.6 |
10 |
80 |
3.0 |
BRMGe-26 |
48 |
26 |
2.5 |
16 |
40 |
1700 |
|
2.2 |
|
|
2.2 |
2.2 |
|
| 镁尖晶石锆砖 |
| MLSZ-93A |
96 |
5 |
0.7 |
1 |
1-3 |
17-18 |
2.85 |
50 |
1700 |
|
12 |
100 |
3.0 |
| MLSZ-93B |
88 |
5 |
0.8 |
2.5 |
1-3 |
17-18 |
2.8 |
50 |
1600 |
|
10 |
80 |
2.9 |
| 镁尖晶石砖 |
| MLFS-R63A |
85 |
3 |
7.5 |
0.9 |
|
16-17 |
3.0 |
50 |
1660 |
|
10 |
100 |
2.5 |
| MLFS-R63B |
80 |
3 |
7.5 |
2.0 |
|
16-17 |
2.9 |
45 |
1630 |
|
8 |
80 |
2.5 |
| 铝镁尖晶石锆砖 |
| AMB-90 |
5.0 |
90 |
0.6 |
0.8 |
|
18 |
3.15 |
90 |
1700 |
±0.5(1600°C×2h) |
|
|
| AMB-80 |
5.0 |
85 |
1.2 |
|
|
18 |
2.95 |
70 |
1650 |
±0.5(1500°C×3h) |
|
|
| UAM |
5.0 |
80 |
|
|
|
16 |
2.9 |
60 |
1600 |
±0.6(1500°C×3h) |
|
|
|